Also depending on who's hot band was used the fatigue performance of the materials will differ due to differing inclusion content and morphology.
I couldnt find a data sheet on the Uddeholm 716, I do know that the Sandvik 7C27Mo2 is a modified 420 stainless (basically 420ss + 1.0%wtMo) has a UTS>250+ksi, and relatively low numbers of large non-metallic inclusions. And generally low numbers of inclusions all together....
I'd bet that the Uddeholm material is similar (if its stainless) If its carbon steel then its likely of the 1095 variety.