I have conducted coupled field analysis using ANSYS, to simulate 3D welding and to find its residual stresses. I have used physics option and calculate separately the thermal problem and structural problem.i import the temperatrues from the thermal analysis for structural analysis .I have calculated the residual stress , But I found the maxcimal residual stress are higher than the yield stress (about its 1.6 times) ,and von Mises stress exceed the yield stress too.i have defined the yield stress in different temperatrue and define the plastic behavior.
its residual stress may be exceed the yield stress a little,
but it is too large
why?would you tell me the reasons
thinks a lot
james