I have been tasked with modifying a cast aluminum part and I am trying to match metals as closely as I can. I need to machine a new part to weld onto this casted part. Our metal scanner gave me a read out of:
alloy 1: 384/80/19
Zr 0.003 +-0.001
Ta 0.024 +-0.007
Fe 0.117 +-0.016
Al 90.648 +-0.401
Si 9.200 +-0.304
What off the shelf aluminum alloy best matches what I have?
Thank You for your help
Jerry