HELP FINDING A SUITABLE METEL FOR METHANOL SUBMERSION

Status
Not open for further replies.

bob1111

Aerospace
Oct 14, 2008
68
We have an automotive fuel system part we need to machine that will be subject to 99% Methanol. We are open to nearly any metal as long as it has a high level of machinability and is not an exotic (expensive) material. We have considered 300 series stainless and a few Brasses. The OEM part we are replacing is brass but known for corroding over time.

Can someone point us in the right direction for a material selection that will machine nice, is relatively inexpensive, and will perform well in Methanol? We do not need 100% corrosion resistance but an improvement over the OE parts is a must.
 
Replies continue below

Recommended for you

I would like to add that I would really like to learn what elements actually cause this reaction so maybe it can help us refine our search. I know Aluminum is very bad with Methanol and does not hold up well.

We also will need to stay with metallic materials due to this being a metering valve.
 
viper,
The Outokumpu's Corrosion Handbook is listing all the austenitic stainless steels as suitable for methanol environment (100% @ 65 deg C - boiling point!), with less than 0.1 mm/year corrosion rate. In fact, that's equivalent to almost 0 mm corrosion allowance or using Outokumpu's words, 'corrosion proof'. You can also visit the Outokumpu website and order your own free famous Corrosion Handbook (there are quite a few other similar books on the internet from other sources).
Cheers,
gr2vessels
 
That is interesting. Do you show any other materials that perform as well but would have a higher level of machinability?
 