Requirements:
  • >500°C heat resistance
  • Nonconductive
  • Able to seal, or non-porous if needed
  • Won’t dissolve in water when cured
  • Consumer-accessible; no materials I need to buy in bulk for a factory
For context; I’m working on developing a concept for a new engine. I need something similar to a glow plug that can go on the end of a brass cylinder 6mm wide inside. No glow plugs I’ve found are this small, and I also need it to be heated constantly.

So far, I’ve tried putting resistive wire into clay on the end of the cylinder, however it seems to crumble too easily and not seal well. Epoxy would be perfect, but it can’t handle high temperatures. Silicone may work but it’s flammable, it’s also hard to get to stay in place in my application.

Also, I’m doing this all with basic tools. My methods of machining are a $40 Amazon mini wood lathe and a pair of calipers. I can’t use anything like steel.

Any eng tips are appreciated!
 
Last edited:
Spark plugs use ceramic bodies
Thought about that, that’s what I was trying with clay. Might need to make some proper ceramic to test it, a bit difficult to do at home though.
 
Last edited:
You need to fire it at a high enough temperature to vitrify it. You may be able to do this with a small propane torch considering the small size of your part.
 
I thought quartz mortar. If you can find quartz sand, mix with Portland cement . This material will resist to temperature , wearing and has low thermal expansion.
 
I thought quartz mortar. If you can find quartz sand, mix with Portland cement . This material will resist to temperature , wearing and has low thermal expansion.
I never thought of that, this might be perfect. I live in Florida and work at a hardware store, so I could pretty easily get free beach sand (which is mostly quartz here) and collect cement dust. Likely too impure though, either way this is a great idea. May end up trying it properly too.

Edit: Gah, it’s porous when dried.
 
Last edited:
You need to fire it at a high enough temperature to vitrify it. You may be able to do this with a small propane torch considering the small size of your part.
Rightttt, “air drying” isn’t the same as firing. I’ll try this and see if I can get it to solidify better. Thanks!
 
I never thought of that, this might be perfect. I live in Florida and work at a hardware store, so I could pretty easily get free beach sand (which is mostly quartz here) and collect cement dust. Likely too impure though, either way this is a great idea. May end up trying it properly too.

Edit: Gah, it’s porous when dried.

It is worth to try. As far as i know , it is not porous. I will suggest a mix design by weight: 1 water+ 2 cement+ 3 quartz sand.
 
Have you tried those little ceramic resistor tubes you can find in old electronics? They can handle crazy heat and might be just the right size for your 6mm brass cylinder. Just wrap your nichrome wire around one and seal it in with some high-temp RTV (the red stuff). Not perfect, but it's held up for me in similar situations.
 
Have you tried those little ceramic resistor tubes you can find in old electronics? They can handle crazy heat and might be just the right size for your 6mm brass cylinder. Just wrap your nichrome wire around one and seal it in with some high-temp RTV (the red stuff). Not perfect, but it's held up for me in similar situations.
You know what, that might be perfect. I have one lying around from a broken 3D printer nozzle. Great thinking! I believe it’s exactly 6MM in diameter and has a brass casing.
 
Would this work?

Potentially, I hadn’t been able to find one of those that mentioned the exact size, thanks! The low voltage isn’t ideal for me but I could make it work, was looking for more like 12V. Would also have to trim down the plug slightly since 1/4” is a little over 6mm.
 
I googled "nonconductive refractory ceramics for temperatures above 500 C" and came up with several that including zirconia and alumina. Macor (mentioned above) sounds like it fits the bill in part because it is machinable. Characteristics include:

  • High Use Temperature: Continuous use up to 800 °C (1472 °F) and peak temperatures up to 1000 °C (1832 °F).
  • Excellent Electrical Insulator: Good electrical insulation properties.
  • Machinable: Can be machined with ordinary metalworking tools, which can be advantageous in certain applications.
  • Other Features: Low thermal conductivity, strong, rigid, and radiation resistant.

Mullite is good in electronics and structural applications and has
  • High Thermal Resistance: Withstands temperatures up to 1700 °C (3092 °F) in air atmosphere.
  • Good Electrical Resistivity: Suitable for applications requiring electrical insulation.
  • Other Features: High creep and corrosion resistance, low thermal expansion coefficient, and good thermal shock resistance.
 
Cheap and readily available -

Less cheap

 