Hello!! I need to help with Equivalence ASTM And DIN.

Is Equivalent ASTM A105 With DIN St37.2???

Is St37.2 available for Temperatures of 450 ºC??

Please Help

Thank in advance. Bye
 
Replies continue below

Recommended for you

You can find a correspondence table in


See also


St37.2 is given as equivalent to ASTM A 283 Gr. C

You should be cautious with correspondence tables.
In principle all the paragraphs and requirements should be checked in both materials to substantiate equivalence.

Low carbon steel is not supposed to be employed at 450 C.

 