I have always used the Wahl Stress correction factor. There are at least two others: Sopwith and Bergstraesser. Does anyone have the formulas for these? What are the differences, strengths, weakness, etc?
 
Replies continue below

Recommended for you

Found my own answer perhaps

Sopwith: (c + 0.2)/(c-1)

Bergstraesser: (c + 0.5)/(c-0.75)

Bergstrasser might be a little more accurate at low spring indexes. With spring indexes above 3, all should are similar enough for my needs
 
Glad to hear you were able to find an answer and thanks for checking back in and letting everyone know.