In looking at the attached boring log for the east coast area where the water table is about 2.5’ below surface, I was considering helical piles and grade beams but the client is saying that the local engineers use strip and spread footings for the residential buildings. The loading would be about 2,500 plf of wall.
My concern is mostly settlement since the soil has very low blow counts. The house will be built on 10” concrete walls that would be 8’ above ground. The bottom of footing has to be 3’ below grade.
I was interested to see what others think. Also, wouldn’t we get more bearing capacity out of the soil since the weight of concrete foundation wall can consolidate the poor layers? Is there a way to estimate the capacity of the consolidated soil in this case? Any suggestions is greatly appreciated.
My concern is mostly settlement since the soil has very low blow counts. The house will be built on 10” concrete walls that would be 8’ above ground. The bottom of footing has to be 3’ below grade.
I was interested to see what others think. Also, wouldn’t we get more bearing capacity out of the soil since the weight of concrete foundation wall can consolidate the poor layers? Is there a way to estimate the capacity of the consolidated soil in this case? Any suggestions is greatly appreciated.