What are the recommended materials for wetted helical compression springs in hydrogen service? I've read that Elgiloy and MP35N are good. What about Inconel X-750 with precipitation heat treatment (4 hours @ 1200F)? Any others?

Thanks!
 
'Hydrogen service'...

Room temp? High temp? Cryogenic?

Pure H2... or compounds of hydrogen H**['sour']?

Regards, Wil Taylor
o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 
Pressure - up to 1500 psi
Temperature - 0 to 120F
Hydrogen concentration - 5% to 100% with the balance being clean natural gas

Thanks!
 
Inconel 718 might also be an option. It is used for critical fasteners in nuclear, so it has been studied to death.