I have a requirement for a Nichrome heat seal blade which is used to heat seal & cut a polythene bag. The problem I hope somebody could assist me with is the maximum heating of the blade under fault conditions, what temp will it reach ? or will it 'pop' like a fuse ?
Blade details
Material - Nichrome 80/20
Size - 65mm x 30mm x 0.5mm
Electrical resistivity @ RT - 108Microhm/cm
Temp coefficient of Resistivity - 100ppm/°C (25° to 105°C)
Thermal conductivity @ 100°C - 15.0W/múK
Supply 110vac
Blade details
Material - Nichrome 80/20
Size - 65mm x 30mm x 0.5mm
Electrical resistivity @ RT - 108Microhm/cm
Temp coefficient of Resistivity - 100ppm/°C (25° to 105°C)
Thermal conductivity @ 100°C - 15.0W/múK
Supply 110vac