Sep 5, 2014 #1 ledon Marine/Ocean Joined Jun 24, 2003 Messages 63 Location US Looking for the reference materials on general heat treatment techniques and basic parameters for metals. This is to help educate someone without and engineering background. Any suggestions?
Looking for the reference materials on general heat treatment techniques and basic parameters for metals. This is to help educate someone without and engineering background. Any suggestions?
Sep 5, 2014 #2 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US Metallurgy for the Non-Metallurgist is available from ASM International in various forms: online class, on-site class, book, DVD ... Go to the ASM site (http://www.asminternational.org/) and type non-metallurgist in the search box. Then choose the product that most suits your needs. Upvote 0 Downvote
Metallurgy for the Non-Metallurgist is available from ASM International in various forms: online class, on-site class, book, DVD ... Go to the ASM site (http://www.asminternational.org/) and type non-metallurgist in the search box. Then choose the product that most suits your needs.
Sep 5, 2014 #3 EdStainless Materials Joined May 20, 2004 Messages 16,351 Location Waukesha WI USA And they have a steel heat treating course also. Great place to start. = = = = = = = = = = = = = = = = = = = = Plymouth Tube Upvote 0 Downvote
And they have a steel heat treating course also. Great place to start. = = = = = = = = = = = = = = = = = = = = Plymouth Tube