alliedtrans
Automotive
Hello I am new to the forum and had a couple of questions:
1. What should be the case depth for gears which are fitted in the Corolla Car and Minivan gearbox as I am receiving complaints of broken gears. i used 20MnCr5 with a CD of .8 to 1mm. Should I used EN 353 and if so can someone please tell me the cycle I need to use.
2. I would like to manufacture the attached component and would like inputs as to what the procedure should be to achieve a hardness of 48 to 53 HRC with minimal distortion as straightening for this component is extremely difficult. Material can be EN 8D or 16MnCr5. I know companies using En 8D and using induction hardening with plug quenching.
Any help would be greatly appreciated.
Thanks
Ankur
1. What should be the case depth for gears which are fitted in the Corolla Car and Minivan gearbox as I am receiving complaints of broken gears. i used 20MnCr5 with a CD of .8 to 1mm. Should I used EN 353 and if so can someone please tell me the cycle I need to use.
2. I would like to manufacture the attached component and would like inputs as to what the procedure should be to achieve a hardness of 48 to 53 HRC with minimal distortion as straightening for this component is extremely difficult. Material can be EN 8D or 16MnCr5. I know companies using En 8D and using induction hardening with plug quenching.
Any help would be greatly appreciated.
Thanks
Ankur