StuartReid
Mechanical
Hello, all,
I need help in working with a metal unfamiliar to me. I have a need to machine and heat treat 17.4PH stainless steel and I need to know temperatures, durations, atmospheric requirements. Does anyone have a reference, data tables, or the information off the top of their heads? Please help. Thanks Stuart
I need help in working with a metal unfamiliar to me. I have a need to machine and heat treat 17.4PH stainless steel and I need to know temperatures, durations, atmospheric requirements. Does anyone have a reference, data tables, or the information off the top of their heads? Please help. Thanks Stuart