1. Can 6AL-4V be heat treated to a minimum of 160,000 KSI?

2. If so, how can I calculate what its shear strength
should be for the following case:
Let's say I need to produce a 4" long shaft made from
such material 1/2" in diameter and with a 3/16" hole
drilled end-to-end along its length in the center of
the stock. Thru that 3/16" hole I intend to insert an
11/32" shaft of the same material.

3. What can I expect the rockwell (RC) to be if the
tensile strength after heat treat is 160,000 KSI.
Thanks
 
Replies continue below

Recommended for you

If you enjoy golf, the maxmium hardness (40 HRc) for the solution treated and aged Ti6Al-4V alloy can be found in the article on golf club material in the tech article link at the bottom of the spec sheet mentioned above;

"AEROSPACE ALLOY HAS BEEN A HUGE SUCCESS IN GOLF CLUB DESIGN"


 