Is it possible to laminate the PVC heatshrink film ? looking for Heat shrink film that has a adhesive backed layer
 
PVC heat shrink tubing is commercially available adhesive lined. What you have requested is certainly possible.
 
That is polyethylene and OP has specified PVC.
 