MiketheEngineer
Structural
Please help this poor old structural.
Scenario:
Metal pipe running a process at 900 degreees F
Piece of wood at 6'' from pipe - doesn't matter what kind of wood as all will start charring at about 450-500 F
Ambient air temp is 75 F
No wind
Humidity is say 30%
IS there an equation or table that will tell me at about what temperature the piece of wood will attain?? Obviously I am afraid of fire and wood degradation.
Thanks for any help...
Scenario:
Metal pipe running a process at 900 degreees F
Piece of wood at 6'' from pipe - doesn't matter what kind of wood as all will start charring at about 450-500 F
Ambient air temp is 75 F
No wind
Humidity is say 30%
IS there an equation or table that will tell me at about what temperature the piece of wood will attain?? Obviously I am afraid of fire and wood degradation.
Thanks for any help...