Nov 22, 2002 #1 baglamas Materials Joined Nov 15, 2002 Messages 6 Location CA I can't find anywhere heat of fusion for any grade of steel. I'm interested in low and high carbon steels but any other grade would also be helpful. I would appreciate it if someone could tell me where I could look up this information. Thanks
I can't find anywhere heat of fusion for any grade of steel. I'm interested in low and high carbon steels but any other grade would also be helpful. I would appreciate it if someone could tell me where I could look up this information. Thanks
Nov 22, 2002 #2 TD2K Chemical Joined Jan 11, 2002 Messages 2,629 Location US http://www.engineeringtoolbox.com/MaterialProperties/LatentHeatsOfMelting.htm has some but for cast iron (more range than I'd have expected). A couple of other links that did list steel didn't include a value. I'll check in my CRC reference book tonight. Upvote 0 Downvote
http://www.engineeringtoolbox.com/MaterialProperties/LatentHeatsOfMelting.htm has some but for cast iron (more range than I'd have expected). A couple of other links that did list steel didn't include a value. I'll check in my CRC reference book tonight.
Nov 22, 2002 #3 TD2K Chemical Joined Jan 11, 2002 Messages 2,629 Location US My CRC book "Handbook of tables for Applied Engineering Science" gives the heat of fusion for iron as 65 cal/gm. Sorry, that's not really what you were looking for but it's all I have. Upvote 0 Downvote
My CRC book "Handbook of tables for Applied Engineering Science" gives the heat of fusion for iron as 65 cal/gm. Sorry, that's not really what you were looking for but it's all I have.
Nov 22, 2002 #4 IRstuff Aerospace Joined Jun 3, 2002 Messages 44,902 Location US This exam document has a problem #3 listing heat of fusion as 237 kJ/kg: http://www.me.gatech.edu/jonathan.colton/me6222/f01final.pdf TTFN Upvote 0 Downvote
This exam document has a problem #3 listing heat of fusion as 237 kJ/kg: http://www.me.gatech.edu/jonathan.colton/me6222/f01final.pdf TTFN
Nov 22, 2002 #5 IRstuff Aerospace Joined Jun 3, 2002 Messages 44,902 Location US This one says 271: http://ctklj.ctk.uni-lj.si/kovine/izvodi/mit0234/grozdanic.pdf TTFN Upvote 0 Downvote