2
Is there a defined envelope for heat input in regards to a pWPS in D1.5?
I am familiar with D1.1 and only recently been exposed to D1.5. Since our shop primarily runs FCAW, we will be producing a WPS with supporting PQR for that process. However, for my first run at this, we plan to use SMAW (7018) using a pWPS.
Once this heat input range is defined, will we need to time every pass that the welder does during their test?
 
Replies continue below

Recommended for you

if you look in table 12.3 , 12.4 , 12,5 me by you find your solution .
 
Good morning denlow60,
Thank you for that direction.
 
Status