Dear friends,

For one of S&T heat exchanger (AET type) found leak due to Sour water corrosion. The sour water contains Sulfides, Ammonia and caustic which are creating corrosive environment. However the material of construction of the existing condenser cooler is carbon steel so please advise me 304 SS material is more suitable for this application?

Design temp: 81 Deg C shell side and 76 tube side
Design pressure: 8.6 barg/FV for shell side and 10 BARG /FV for tube side.
service ; SOUR WATER for shell side and COOLING WATER at tube side

Thank you,

regards,
Sameer
 
Replies continue below

Recommended for you

Almost one year now, this exchanger is not in service.
 
please do not double post.
The thread is already active in the B&PV forum

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 