Anyone has photos or sketch showing Fusion Zone and Heat Affect Zone on TIG Weld butt Joint. Thanks
 
Replies continue below

Recommended for you

While the description in the file above is accurate, the image shows the HAZ to be wider than the weld. In reality, it's normally a relatively narrow band whose width depends on heat input, material type and other factors, but for manual GTAW on CS, will probably be < 1/8", and most likely around 1/16".
 