Merzi

Mechanical
Dec 12, 2002
50
We are fabricating a SS vessel. Heads will be hot formed , what type of testing has to be done after forming, and at what temp it has to be hot formed .

Merzi
 
Replies continue below

Recommended for you

I would suggest that you follow the requirements in the ASME B&PV code, Section VIII for unfired pressure vessels. Part UHA of Section VIII contains excellent technical information on solution treatment requirements and NDT regarding forming of austenitic stainless steel materials.
 
More specific information is required to answer your questions. What is the type and grade of material, what is the thickness, is the head of welded two piece construction?
 
Merzi,

Where will this vessel be located and installed ?

What is the design (maximum working)pressure (MAWP) ?

MJC

 