Hello,
I hope someone with experience can clear something up for me.
I'm trying to size required DR for a water pipeline under full vacuum. The pipeline will be buried 3m, and I intend to achieve a soil reaction - E' = 2000-3000 psi through material type and high compaction.
Now, when calculating the DR, if the pipe is considered constrained for the entire length a DR 21 pipe will be suitable and achieve a factor of safety of ~2.5-3 for vacuum / soil prism / live loads relative to critical collapse pressure.
However, if the pipe is considered unconstrained, the external pressure of the vacuum exceeds the critical collapse pressure. In the case of unconstrained pipe, DR 13 would be the suitable choice.
My question is, is it safe to assume through diligent supervision of the construction, and tight specifications for the embedment,and primary / secondary fill, that the DR 21 will be sufficient?
Is it common practice to only consider the pipe under constrained conditions for buried pipelines?
Thank you for any help you can provide.
I hope someone with experience can clear something up for me.
I'm trying to size required DR for a water pipeline under full vacuum. The pipeline will be buried 3m, and I intend to achieve a soil reaction - E' = 2000-3000 psi through material type and high compaction.
Now, when calculating the DR, if the pipe is considered constrained for the entire length a DR 21 pipe will be suitable and achieve a factor of safety of ~2.5-3 for vacuum / soil prism / live loads relative to critical collapse pressure.
However, if the pipe is considered unconstrained, the external pressure of the vacuum exceeds the critical collapse pressure. In the case of unconstrained pipe, DR 13 would be the suitable choice.
My question is, is it safe to assume through diligent supervision of the construction, and tight specifications for the embedment,and primary / secondary fill, that the DR 21 will be sufficient?
Is it common practice to only consider the pipe under constrained conditions for buried pipelines?
Thank you for any help you can provide.