Oct 25, 2019 #1 afox92 Civil/Environmental Joined Oct 25, 2019 Messages 1 Location US A fuser I'm working with tells me that he can't saddle fuse a 16' x 8" branch saddle to a 16" DR17 main HDPE pipe. Is he right or can it be done?
A fuser I'm working with tells me that he can't saddle fuse a 16' x 8" branch saddle to a 16" DR17 main HDPE pipe. Is he right or can it be done?
Oct 25, 2019 #2 jdonville Geotechnical Joined Sep 29, 2003 Messages 985 Location US https://www.centralplastics.com/en_US/gfcp-products2/elec-pe-fittings/elec-saddle.html It appears that the saddles exist, so suggest that you ask for the specific reasoning as to why they are unable. Upvote 0 Downvote
https://www.centralplastics.com/en_US/gfcp-products2/elec-pe-fittings/elec-saddle.html It appears that the saddles exist, so suggest that you ask for the specific reasoning as to why they are unable.
Oct 25, 2019 #3 bimr Civil/Environmental Joined Feb 25, 2003 Messages 9,377 Location US Maybe he doesn't have the equipment to do it. Upvote 0 Downvote