Hi all
I am designing 3d (3 x diameter) & 2d (2 x diameter) bending
press for HDPE pipes, the pipes are heated to 2500 deg C where after they are filled with pellets to keep the pipe's shape during bending, can anyone help me with force required to bend the pipes.The pipes sizes are 110mm up to 1000mm. The pipes are bent tyo 90 deg. Please help
I am designing 3d (3 x diameter) & 2d (2 x diameter) bending
press for HDPE pipes, the pipes are heated to 2500 deg C where after they are filled with pellets to keep the pipe's shape during bending, can anyone help me with force required to bend the pipes.The pipes sizes are 110mm up to 1000mm. The pipes are bent tyo 90 deg. Please help