Hi all,
I’m working in an hydrochloric acid - facility (HCL 37% concentration) at 58C and 1035 KPa. I need to connect my tank to the existing piping.

I have two options to go: centrifugally cast fiberglass or FRP+PVC liner. Dont really have gidelines from Client.

Both vendors are offering the “best product” for the application.

Has anyone had precedent experience (good or bad) with such or similar stream/materials?

Thanks a lot,
 
Replies continue below

Recommended for you

10 bar and 60 C conc acid? The consequences of a spill scare me enough that I'd consider lined steel pipe- more joints and risk of damage from the outside if the acid spills, but also more mechanically robust.

If the linesize is small (less than 3" NPS), stay away from the centrifugally cast FRP. The PVC with FRP overwrap is a better option for smaller linesizes. Make sure that the people doing the work are competent.
 