I'm working on a project of installing a new heavy equipment on the existing roof structure. Roof structure is made of metal deck with insulation and open steel joists are supporting the deck.
Site visit found the existing steel joist is like this in the photo.
It reads 3371138-1J24, VULCRAFT 140.
I researched '75-YEAR STEEL JOIST MANUAL' and website, but I could find NO clue at all about this joist.
I contacted Vulcraft for requesting information of their old joist and I'm waiting.
Using structural analysis program to model and analyze the structural will be another option, you think?
Any good idea or comment are welcomed.
Thank you so much!
Site visit found the existing steel joist is like this in the photo.
It reads 3371138-1J24, VULCRAFT 140.
I researched '75-YEAR STEEL JOIST MANUAL' and website, but I could find NO clue at all about this joist.
I contacted Vulcraft for requesting information of their old joist and I'm waiting.
Using structural analysis program to model and analyze the structural will be another option, you think?
Any good idea or comment are welcomed.
Thank you so much!