1
- #1
Hi,
First time post. I need to fabricate a steam jacket for a butterfly valve from C276 / N10276. I am struggling to find a supplier of plate and pipe / tube. Obviously not helping that I don't need much as it is a 1 - off and only about 370mm DIA
Can anyone help? Preferably UK supply
First time post. I need to fabricate a steam jacket for a butterfly valve from C276 / N10276. I am struggling to find a supplier of plate and pipe / tube. Obviously not helping that I don't need much as it is a 1 - off and only about 370mm DIA
Can anyone help? Preferably UK supply