Apr 18, 2011 #1 robertolourdes Mechanical Joined Apr 3, 2011 Messages 2 Location AU any ideas how to machine a cast hastelloy 276, milling ( face and end mill), drilling and tapping. Cutter types, speeds and feeds.
any ideas how to machine a cast hastelloy 276, milling ( face and end mill), drilling and tapping. Cutter types, speeds and feeds.
Apr 18, 2011 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US The producer of Hastelloy C-276, Haynes International, has some information available in the following document: http://www.haynesintl.com/pdf/h2010.pdf Upvote 0 Downvote
The producer of Hastelloy C-276, Haynes International, has some information available in the following document: http://www.haynesintl.com/pdf/h2010.pdf