Hee Fellow engineers,

I would like to know if someone ever used the Chaboche model in FEM, preferably MSC.MARC. I want to use the bauschinger effect in my FEM models.

Thanx

BuckTU
 
Unless you need rate-independence for something else, you don't need Chaboche just for the Bauschinger effect, so use a general kinematic hardening model instead, it's much easier to set up.


------------
See faq569-1083 for details on how to make best use of Eng-Tips.com
 
I believe that you can combine the Chaboche model with other material models, to include the effects of strain hardening/softening, although I have not done it yet myself.

I have found that the Chaboche non-linear material model can predict greater ratchetting than an equivalent multi-linear kinematic hardening model under cyclic loading conditions.
 