Hi all,

HARDOX is a commercial name. What is the steel name for HARDOX 400/500 ? (I can't find on their web site. )
And what is the density for HARDOX 400/500 ?
Thanks for feedback.

Best.
JNB
 
Here is the HARDOX web site with product information. The HARDOX 400 or 500 is considered abrasion resistant plate.


Look for the data sheets at the bottom of the web page.

The density for this material is similar to steel;
.27 lbs/cubic inch
 
What are the other wear resistant plates with similar
mechanical properties to HARDOX400 on the market ?
I guess RAEX AR400 from Finland is one of them.

--JNB
 