Hi,

I need to bend Hardox 500 to an angle of 35 deg. Material thickness is 30 mm, bending length is 75 mm. What would be the most econonmical bending method using a shop 200 ton press.

Thanks
 
Replies continue below

Recommended for you

Thank you metengr,

I tried doing it as specified in the attachment, It always get cracked, Do you think I need to reheat it prior to bending it.
 
thwainy;
Contact the technical guys at Hardox based on the link I provided. They will help you.
 
Metengr,

Thanks so much, definitely will do that.