ASTM E10-14 (Standard Test Method for Brinell Hardness of Metallic Materials) shows all testing to be done with a tungsten carbide ball (sect. 5.2.3), hence the W is added to all values. The HBW is used for all hardness ranges from 1 to 650 HBW.
If you are not using the standard 10mm ball and 3000 kg load, and 10-15 second dwell time (10/3000/15), then you must also list the ball diameter, load, and dwell time following the 'HBW' when expressing a result. It would be a good idea for you to purchase a copy of this ASTM standard for your reference.