Gentlemen,
I working on the project that require to do hardness test after PWHT but the project spec doesn't give a acceptance criteria.
Where can I get the hardness valve for SA 106, SA 335 P11, SA 335 P22. I checked into ASME Sect II but can not find the hardness value.
Thank you.
Ittichet
I working on the project that require to do hardness test after PWHT but the project spec doesn't give a acceptance criteria.
Where can I get the hardness valve for SA 106, SA 335 P11, SA 335 P22. I checked into ASME Sect II but can not find the hardness value.
Thank you.