We are in need of a good hardness tester. It will need to do about 300 Rockwell C hits a day + the occasional R15N.

We are looking at the NewAge Indentron. Cost is about $17k.

Does anyone have any experience with this one or others?

TIA
 
Replies continue below

Recommended for you

I have had good luck with the Indentron in a high volume met lab environment for QC checks. We had one in the lab and two or three on the shop floor and they held up fine.
 
The Instron Wilson Rockwell 2000 is a much better instrument than the Indentron. I have used both instruments extensively, and I highly recommend you spend your money on the 2000 instead.
 
The Indentron has worked well in my lab with no issues but I was hesitant to use it on the heat treat shop floor. For a high volume of HRC tests I would recommend Newage's (now Ametek) Versitron with the auto foot pedal option.

I also agree that the Instron 2000 is a very good machine.

Struers has a new DuraJet benchtop machine, with load cell technology like the Instron and clamping capability for about $22k.
 
I am also a big fan of the Wilson Rockwell 2000 from Instron. It is extremely easy to use, with excellent accuracy/precision.
 