johnthebest
Mechanical
Hello everyone
I would like to have your help about this technical query
In our project specification, we said the following:
when required, hardness test shall be performed on.... "see page 3 of 3 in the attached file"
The contractor is proposing the following:
For P1 material weld and HAZ with PWHT hardness values shall be 200 BHN max.
For P1 material weld and HAZ without PWHT hardness values shall be 237 BHN max.
and the justification is given in page 1&2 of the attached file
Now what I want to understand: what does it mean "when required" in the spec and is there any deviations from what the contractor is proposing.
Thx in advance
I would like to have your help about this technical query
In our project specification, we said the following:
when required, hardness test shall be performed on.... "see page 3 of 3 in the attached file"
The contractor is proposing the following:
For P1 material weld and HAZ with PWHT hardness values shall be 200 BHN max.
For P1 material weld and HAZ without PWHT hardness values shall be 237 BHN max.
and the justification is given in page 1&2 of the attached file
Now what I want to understand: what does it mean "when required" in the spec and is there any deviations from what the contractor is proposing.
Thx in advance