Hi,
In my company we have a internat standard that recommends to do a hardness test after PWHT in the HAZ and in the weld, obviously to evalute the PWHT, but we have to compare these values with some standard value of maximum hardness after PWHT. I only found this kind of rereference in ASME B31.3 but not for P-number 1 materials which I'm interested in. Do you know any literature or standard where I could find this information?
Thanks a lot.
In my company we have a internat standard that recommends to do a hardness test after PWHT in the HAZ and in the weld, obviously to evalute the PWHT, but we have to compare these values with some standard value of maximum hardness after PWHT. I only found this kind of rereference in ASME B31.3 but not for P-number 1 materials which I'm interested in. Do you know any literature or standard where I could find this information?
Thanks a lot.