metboss
Petroleum
- Sep 12, 2012
- 153
Hi all,
For L-80 pipe raw material, certifcates shows through wall hardness value within the acceptable limits of API 5CT (9th ed) i.e. 23 HRC whereas surface hardness mentioned 24 HRC(more than API 5CT limit).
Can we accept this based on through hardness value or we should consider both??
Regards
For L-80 pipe raw material, certifcates shows through wall hardness value within the acceptable limits of API 5CT (9th ed) i.e. 23 HRC whereas surface hardness mentioned 24 HRC(more than API 5CT limit).
Can we accept this based on through hardness value or we should consider both??
Regards