A simple question on case hardening.
A part casted with 1020 steel, but need carburize ( .012 MIN DP) to HRC 30~45 in case. My questions are:
1. Can we test the hardness with HRA or superficial scale and convert it to HRC?
2. The size in section is 3/8” square, if hardness in surface measured at HRC 40, what is the hardness in core ?
3. If the hardness measured at HRC 15 in core, is this a carburizing process ? If not, what is the possible processing in heat treatment.
Thanks for all inputs
SeasonLee
A part casted with 1020 steel, but need carburize ( .012 MIN DP) to HRC 30~45 in case. My questions are:
1. Can we test the hardness with HRA or superficial scale and convert it to HRC?
2. The size in section is 3/8” square, if hardness in surface measured at HRC 40, what is the hardness in core ?
3. If the hardness measured at HRC 15 in core, is this a carburizing process ? If not, what is the possible processing in heat treatment.
Thanks for all inputs
SeasonLee