Can any one please guide me on the following queries:
1. Our hardness of the subject tube is 100 HRB but code says it should be maximum 90 HRB. Is there any acceptable range other than defined?
2. The tensile for the same sample is coming 977 Mpa. Does tensile strength increase with increase in hardness?
3. Is there any way of single tube hydrotest for heat exchangers given in ASME or TEMA?