Hardness conversion program 5

Status
Not open for further replies.

rayband

Materials
Joined
Apr 10, 2006
Messages
24
Location
US
Does anyone know of a downloadable hardness conversion program (as opposed to conversion table) where one can enter a Knoop or Brinell and get the RC or RB calculated conversion? We shouldn't have to squint at a table then mentally interpolate in this day & age.

RAYBAND
Rock Island Arsenal
AMSTA-RIA-SEM
 
No, you shouldn't have to squint at a table.
You shouldn't be converting hardnesses at all. They don't convert unless you have done the tests with the same materials. And even then you had better not extrapolate.

= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
 
The Uconeer program is neat. It has the most different terms I've seen on one of these programs.

I agree that you have to be careful when using hardness conversions, especially when converting between micro, superficial, HRC, and Brinell. You have to take into account the microstructure you're testing especially if it's not homogeneous.

In the heat treat shop conversion is a valuable diagnostic tool in troubleshooting hardness problems on parts. So I can't discount conversions completely.
 
Thanks dbooker630. I had this program downloaded some years ago but had forgotten about it. It is neat. But I am looking for the conversion equation(s) used so I can put them in a spreadsheet to convert case depth microhardnesses to the HRC values called out in the spec. I could slog through writing the equations myself, but why should I when many others have already done it.

Sorry EDStainless, we all know the gospel, but hardness conversions are a fact of life.

RAYBAND
Rock Island Arsenal
AMSTA-RIA-SEM
 
rayband,

You can find a great deal of information, including conversion equations and uncertainty analysis, in ASTM E 140 and ISO 18265.
 
Thanks TVP. I am aware of those specs and the equations in E 140, but many people including those who write the software for all microhardness hardware and many others have already done that. I am just lazy; I hate to have to spend time doing (redoing, really) what so many others have already done. Knowing that those equations have been written into software so many times for so many years by so many people (including the Uconeer conversion program), it just grinds me to have to do it myself. To me it is like having to forge your own hammer from bar stock just to drive a nail. How much engineering time is wasted having to do relatively menial tasks that many others have already done just because it is not available to you? This is why eng-tips fora is so exciting and valuable to us. Thanks to all.

RAYBAND
Rock Island Arsenal
AMSTA-RIA-SEM
 