One of my project pipe spool required PWHT & production hardness test.The material for Pipe spool was A105/A106 GrB (sch STD)& NACE MR0175 was specified on spool drawing.
The base metal hardness for A105 was 155-160BHN & for pipe A106 GrB was 135-138 BHN before fabrication.
After welding & PWHT(stress relieving at 620 deg C for 2hrs)the hardness for A 105 was 111-120 BHN & that of for A 106 GrB was 102-108 BHN.The weld hardness was between 175-180 BHN.
Now the customer is not accepting the material by saying that UTS for A106 GrB may have dropped below to its min requirement.
What is the minimum acceptable base metal hardness for above two material after PWHT?
how to handle this situation. I am confused????
A quick reply is appreciated.
The base metal hardness for A105 was 155-160BHN & for pipe A106 GrB was 135-138 BHN before fabrication.
After welding & PWHT(stress relieving at 620 deg C for 2hrs)the hardness for A 105 was 111-120 BHN & that of for A 106 GrB was 102-108 BHN.The weld hardness was between 175-180 BHN.
Now the customer is not accepting the material by saying that UTS for A106 GrB may have dropped below to its min requirement.
What is the minimum acceptable base metal hardness for above two material after PWHT?
how to handle this situation. I am confused????
A quick reply is appreciated.