Oct 23, 2003 #1 bruv Materials Joined Feb 19, 2002 Messages 239 Location GB We have some hardfacing to be done with Stellite 6, and I have to develop the procedure. Is there anywhere in ASME IX that covers this sort of thing? Has anybody out there had to do this before? Thanks
We have some hardfacing to be done with Stellite 6, and I have to develop the procedure. Is there anywhere in ASME IX that covers this sort of thing? Has anybody out there had to do this before? Thanks
Oct 23, 2003 #2 GRoberts Materials Joined Apr 22, 2002 Messages 548 Location US ASME IX covers everything you have to do to qualify a hardfacing WPS. Start at QW-216 and go from there. Upvote 0 Downvote
ASME IX covers everything you have to do to qualify a hardfacing WPS. Start at QW-216 and go from there.