I would greatly appreciate if anyone can help me with the following problem we are having with regards to pre-preg handling and lay-up.
We at present place the pre-preg in the freezer for a few minutes just before to be able to remove the backing of the pre-preg otherwise under ambient temperature we are struggling like crazy and distorting the pre-preg material when trying to remove the backing on either side of the pre-preg.
Not only that but when it comes to laying up the pre-preg we are finding it extremely difficulty moulding it around the mould tools as it is so tacky (even though we are doing it in a temperature controlled clean room). Also to mould the pre-preg around the mould tools keeping the one layer of backing on stops the material from moulding into the small grooves in the tool. We are tempted to resort to using barrier cream just so it makes the job easier but I understand that as introducing contaminents into the pre-preg which could alter the properties of the material.
If any one knows of any ways we can overcome the above problems I would greatly appreciate it. Any suggestions and ideas welcome. Thank you
We at present place the pre-preg in the freezer for a few minutes just before to be able to remove the backing of the pre-preg otherwise under ambient temperature we are struggling like crazy and distorting the pre-preg material when trying to remove the backing on either side of the pre-preg.
Not only that but when it comes to laying up the pre-preg we are finding it extremely difficulty moulding it around the mould tools as it is so tacky (even though we are doing it in a temperature controlled clean room). Also to mould the pre-preg around the mould tools keeping the one layer of backing on stops the material from moulding into the small grooves in the tool. We are tempted to resort to using barrier cream just so it makes the job easier but I understand that as introducing contaminents into the pre-preg which could alter the properties of the material.
If any one knows of any ways we can overcome the above problems I would greatly appreciate it. Any suggestions and ideas welcome. Thank you