Last in April, 2004 a question was raised concerning a hammering in a kettle reboiler on the steam side. Many members such as Monetmayor, 25362, sshep, and many others helped troubleshooting this problem.
In this thread I will go through the following points:
1) thanks for all members who helped troubleshooting this problem.
2) The original thread was removed for some reason and can not be retrieved. Sorry!!!
3) The reason behind the hammering was the partition in the channel head found sheared off. This damaged partition plate allowed for steam-condensate contact which resulted in hammering.
4) I have pictures of this sheared off partition plate. Also, Monetmayor prepared excellent sketch of a well designed trouble-free reboiler should look like. If any one is interested to see the pictures and Monetmayor's work on the reboiler, please E-mail me at
trebor10@mail.com
Thanks all
In this thread I will go through the following points:
1) thanks for all members who helped troubleshooting this problem.
2) The original thread was removed for some reason and can not be retrieved. Sorry!!!
3) The reason behind the hammering was the partition in the channel head found sheared off. This damaged partition plate allowed for steam-condensate contact which resulted in hammering.
4) I have pictures of this sheared off partition plate. Also, Monetmayor prepared excellent sketch of a well designed trouble-free reboiler should look like. If any one is interested to see the pictures and Monetmayor's work on the reboiler, please E-mail me at
trebor10@mail.com
Thanks all