HELLO ALL:
I have seen several light airplanes (Cessnas, pipers, etc) with hail dimples. I have HEARD that the hail dimples can be removed by palcing dry ice over the dimple.

Is this true? If not is their a method other than reskinning?

Regards
Dave
 
Replies continue below

Recommended for you

Dry ice doesn't make any sense at all.

How big are the dimples?

Steven Fahey, CET
 
SPARWEB: Thanks for the response. The dimples I have seen are in round numbers .75 to 1 inch across and maybe 1/16" - 1/8" deep. It depends on the particular hailstorm they are in.

Regards
Dave
 
If you can afford it, try electomagnetic dent removal, there was a post somewhere on this forum about that.
B.E.
 
Aviat's link at airstream mentions the people I was trying to think of.
For more detail goto thread 120-706 on this forum.
B.E.
 
Forum 2 thread 120706 Electromagnetic Dent removers-Advice
Currently on page 6 of the forum. For some reason I cannot get the search engine to locate it But thats where it is.