Hi all
we have some H_Exchenger in NACE MR0175 condition.
Tube is S.S. 316L & Tube Sheet is C.S.(A-105).
Tubes double expanded & seal weld to tube sheet.
electrode is E-309 & W.P.S. is `nt content PWHT.
but impacted & 200 brinel is it`t hardness.
in start up seal weld is cracked & leak from them.
Please explain me What is the matter?is PWHT mandatory?