Hello,
I have a commodity with a concentration of 0,5% of H2S04 and a temperature of 200ºC, and, I don't know if this concentration is very acid.
Someone can help me??

Thanks,
 
You would consider this a weak acid, but under certain conditions it could be very corrosive especially at your temperature.

One needs a little more information to give any advice.

Is the 0.5% based on vol or weight?

What form is the commodity?

What are the other ingredients?

What do you hope to accomplish?

 
Sorry,

0,5% vol; liquid; water.

I have to specify the material of piping.

Thanks,
 
Is there any chloride in the system? Even a few ppm could be a killer.
Look here for good tips
I would suggest that you look at duplex stainless grades, but you are going to need a high alloy material for any real durability at that temperature.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 