Hello folks.
I am not a metallurgist, so I am looking for some opinions on what to do in a produced water environment in which you have all four of these hypothetical but representative conditions:
(1) it is NACE sour
(2) it has measurable CO2
(3) it has chlorides above, say, 1000 ppm
(4) 2000 psig @ ~75 F
I see a lot of clients asking for ASTM A312 TP316/316L in such service. My thoughts are:
High PREN is good to address the CO2; H2S resistance probably good; not sure that I like the 1000 ppm chlorides with this metallurgy.
Might try Duplex SS...at a cost.
I think the optimum approach is to use internally coated carbon steel with something like a baked fusion bond epoxy.
Also, I have seen aluminum-bronze valves in such service...not sure I like such metallurgy in a NACE sour environment although I have been told that NAB offers acceptable resistance. In any case, I would propose an internally coated carbon steel valve and maybe try Impreglon.
Can anyone provide any thoughts / opinions?
Thanks all in advance.
Regards,
SNORGY.
I am not a metallurgist, so I am looking for some opinions on what to do in a produced water environment in which you have all four of these hypothetical but representative conditions:
(1) it is NACE sour
(2) it has measurable CO2
(3) it has chlorides above, say, 1000 ppm
(4) 2000 psig @ ~75 F
I see a lot of clients asking for ASTM A312 TP316/316L in such service. My thoughts are:
High PREN is good to address the CO2; H2S resistance probably good; not sure that I like the 1000 ppm chlorides with this metallurgy.
Might try Duplex SS...at a cost.
I think the optimum approach is to use internally coated carbon steel with something like a baked fusion bond epoxy.
Also, I have seen aluminum-bronze valves in such service...not sure I like such metallurgy in a NACE sour environment although I have been told that NAB offers acceptable resistance. In any case, I would propose an internally coated carbon steel valve and maybe try Impreglon.
Can anyone provide any thoughts / opinions?