can anyone help me with this heat treatment? what is the standard where all these heat treatments are given?
 
Edstainless is right though 17-7PH carries the TH, RH, OR CH conditions. AMS2759/3 covers the heat treatment of most PH stainless. I'm guessing you are dealing with 17-4, 15-5 or PH13-8MO.
 