Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Gusset Plate Weld Design 1

Status
Not open for further replies.

dik

Structural
Apr 13, 2001
26,063
Is there a good design example that shows the weld design for a gusset plate similar to that shown? The gusset will be welded in place; it's an existing structure.

Gusset_drnon1.png


The a' and b' are the distances to the beam and column centroids

Rather than think climate change and the corona virus as science, think of it as the wrath of God. Do you feel any better?

-Dik
 
Replies continue below

Recommended for you

AISC design guide 29 has plenty helpful examples.

The general gist goes determine a set of admissible forces using uniform force method (or other equilibrium based method), work out average weld stresses under the vertical and horizontal forces on beam and column gusset faces, multiply by ductility factor of 1.25 and design weld for that.

 
Thanks Agent... got it... I was using the KISS method without knowing it was that. I'll take a look to see how the other methods compare.

Rather than think climate change and the corona virus as science, think of it as the wrath of God. Do you feel any better?